product name | application | processing & use level | characteristics |
sa516 | pigment dispersant |
□ incorporated into formula before extrusion
□ 0.5-1% by weight of total formula |
■ good pigment dispersing ability
■ provide better color strength |
k7005 | anti-yellowing agent | □ extruded after premixing, the dosage is 0.3-1% of the total weight of the formula |
■ for a variety of powder coating systems, especially haa systems
■ can significantly inhibit the yellowing of powder coatings caused by gas baking or electric baking |
k7301a | bonding additive | refer to the tds |
■ improve the metal effect of coatings
■ increase bonding temperature and anti caking ■ reduce the dosage of metal pigments |
sa5501 | stabilizer for metal pigment |
□ dry blend
□ 2-3% by weight of total formula |
■ inhibiting from blackening, spot-formation and loss of brilliance of metallic coatings
■ improve heat resistance |
sa5502 | dry powder flow additive |
□ dry blend
□ 0.1-0.5% by weight of total formula |
■ improving fluidity of coating powders
■ anti caking ■ enhancing electrostatic spray efficiency ■ controlling film thickness for thin coating |
k7921 | adhesive modifier | extruded after premixing, the dosage is 0.8-1.5% of the total weight of the formula | improve the adhesion of the coating to metal substrates such as stainless steel and galvanized sheet, improve the flexibility of the coating without affecting the weatherability |
k7010a | special anti-caking additive | □ dry blend □ 0.2-0.4% by weight of total formula | ■ anti caking ■ for almost all kinds of powder coatings ■ improving fluidity of coating powders |
k7658 | surface wetting modifier | □ incorporated into formula before extrusion □ 0.5-2% by weight of total formula | good pigment and filler wetting and dispersing properties and allow to increase the amount of pigment and filler. good wetting performance, improve the coating fog, improve the clarity and freshness of the coating. |
k7771 | wear-resistant agent | □ incorporated into formula before extrusion □ 0.2-0.5% by weight of total formula | can form a coating with excellent wear resistance. especially suitable for sand texture formula. |
k7004 | anti-yellowing agent | □ extruded after premixing, the dosage is 0.5-1.5% of the total weight of the formula | significantly improving discoloration and performance deterioration because of gas baking ; can be used in pes/tgic and pes/h aa systems, etc. |
k7007 | anti-yellowing agent | □ extruded after premixing, the dosage is 0.2-1% of the total weight of the formula | can significantly inhibit yellowing of powder coating caused by electric baking and gas baking. can significantly inhibit the aging of the powder coating caused by high temperature baking, can withstand high temperature baking at 220-250 ℃. |
k7010b | anti caking agent | □ dry blend □ 0.1-0.4% by weight of total formula | significantly improve the dry powder fluidity and construction no harm to the leveling and mechanical properties of the coating. |
k7923 | adhesion promoter | extruded after premixing, the dosage is 0.5-1.5% of the total weight of the formula | significantly improve the adhesion of the coating to special metal substrates such as galvanized, magnesium aluminum alloy; |
products
hotline:
+86-
mobile version
search
add: 15 li dun, north outskirts of luan city, anhui, p, r, china p.c.:237158 | |